Engineering :: Metallurgy
|
|
|
|
|
71. |
Dilute nitric acid applied to a clean fracture of white cast iron will produce |
A. |
White stain |
B. |
Grey stain |
C. |
Black stain |
D. |
Brown stain |
E. |
Pink stain |
|
|
Answer: Option D
Explanation:
|
72. |
Which of the following is not true in case of white cast iron |
A. |
It is whitish in colour |
B. |
It is strong |
C. |
It is hard |
D. |
It is brittle |
E. |
It is malleable |
|
|
Answer: Option E
Explanation:
|
73. |
For acid resistance cast iron should have silicon percentage of |
A. |
1 percent |
B. |
2 percent |
C. |
10 percent |
D. |
15 percent |
E. |
25 percent |
|
|
Answer: Option D
Explanation:
|
74. |
Highest melting point is for |
A. |
Cast iron |
B. |
Wrought iron |
C. |
Mild steel |
D. |
High carbon steel |
E. |
Low carbon steel |
|
|
Answer: Option B
Explanation:
|
75. |
Compressive strength is highest in case of |
A. |
Cast iron |
B. |
Wrought iron |
C. |
Mild steel |
D. |
Low carbon steel |
E. |
High carbon steel |
|
|
Answer: Option E
Explanation:
|
76. |
Ultimate tensile strength is least in case of |
A. |
Cast iron |
B. |
Wrought iron |
C. |
Mild steel |
D. |
Low carbon steel |
E. |
High carbon steel |
|
|
Answer: Option A
Explanation:
|
77. |
Ultimate tensile strength is least in case of mild steel and is of the order of |
A. |
35 - 45 kg/mm2 |
B. |
50 - 60 kg/mm2 |
C. |
60 - 75 kg/mm2 |
D. |
75 - 90 kg/mm2 |
E. |
90 - 100 kg/mm2 |
|
|
Answer: Option A
Explanation:
|
78. |
Welding process used in fabrication of car bodies is |
A. |
Arc welding |
B. |
Resistance welding |
C. |
Thermit welding |
D. |
Brazing |
E. |
Soldering |
|
|
Answer: Option B
Explanation:
|
79. |
The fastest cooling rate is achieved when steel is quenched in |
Answer: Option A
Explanation:
|
80. |
Brass in an alloy of |
A. |
Copper and tin |
B. |
Copper and zinc |
C. |
Copper and lead |
D. |
Copper and nickel |
E. |
Copper and aluminium |
|
|
Answer: Option B
Explanation:
|
Read more:
|
|