Engineering :: Building Materials
|
|
|
|
|
61. |
The natural drying of bricks is also called hack drying. |
Answer: Option A
Explanation:
|
62. |
The indentation marks left on bricks during the process of moulding, are known as |
A. |
fillets |
B. |
frogs |
C. |
projections |
D. |
marks |
Answer: Option B
Explanation:
|
63. |
The frog of a brick is normally made on its |
A. |
longer face |
B. |
shorter face |
C. |
bottom face |
D. |
top face |
Answer: Option D
Explanation:
|
64. |
The average out-turn of first class bricks in clamp burning is about |
Answer: Option B
Explanation:
|
65. |
The average out-turn of first class bricks in kiln burning is |
A. |
50 to 60% |
B. |
60 to 70% |
C. |
70 to 80% |
D. |
80 to 90% |
Answer: Option D
Explanation:
|
66. |
The burning of bricks in kilns is complete within |
Answer: Option B
Explanation:
|
67. |
The bricks after burning in kilns require about |
Answer: Option D
Explanation:
|
68. |
The bricks should be burnt at temperature from |
A. |
300?C to 500?C |
B. |
500?C to 700?C |
C. |
700?C to 1000?C |
D. |
1000?C to 1200?C |
Answer: Option D
Explanation:
|
69. |
The type of briek suitable for panal walls for multi-storeyed buildings is |
A. |
hollow bricks |
B. |
perforated bricks |
C. |
either (a) or (b) |
D. |
none of these |
Answer: Option C
Explanation:
|
70. |
The compressive strength of second elass bricks should bot be less than |
A. |
7.5 MN/m2 |
B. |
9 MN/m2 |
C. |
10.5 MN/m2 |
D. |
12 MN/m2 |
Answer: Option A
Explanation:
|
Read more:
|
|